Blue Demon 5000T - 450mm long x 2.4mm pop pack TIG rod for cast iron repair (8 rods)
· Cast iron repair with minimal or no pre-heat
· Excellent for welding all cast irons
· Welds copper to steel and stainless steel
· Non-Carcinogenic
· No nickel
Suggested settings for Cast Iron Repair:
DC Negative
100 Amps
100% Argon Shielding Gas
2% Thoriated Tungsten with pointed tip
General directions for use on cast iron repair:
For best results use a sparing amount of acetone on a rag and wipe the rod prior to use. If thickness permits, you can “V” out the crack to expose the clean metal. Some TIG welders like to make a quick pass or 2 over the crack to give it a little preheat but also to burn out any grease or oil. Make a puddle with the tip and add filler by a dipping the wire in the puddle. When you complete the weld always leave the weld with a deposit of filler. If the process is not successful, use a magnet to verify that the casting is iron.